Typical Mechanical Properties - Spring Applications
annealing
Heat Treatment: 1950°F (1065°C)
Tensile Strength: 120-160 ksi; (830-1100 MPa)
Tensile Strength: 210-250 ksi; (1450-1725 MPa)
Heat Treatment: After the spring is coiled. Solution Annealing: 1950°F (1065°C) for 4 hours. Age: 1400 degrees Fahrenheit (760 degrees Celsius) for 16 hours.
Tensile Strength: 200-225 ksi (1380-1550 MPa)
Claimed Operating Conditions: -300°F to 1500°F (-184°C to 815°C)
,
Company Profile
Test Equipment :
Company strength:
Certificate:
Welcome to contact us,thanks
Our products sales all over the world as well. From the following two websites you can also get more information about our company:
http://xingda-alloy.en.made-in-china.com
http://xingda-alloy.en.made-in-china.com
Welcome to contact us,thanks
Send your message to this supplier
Find Similar Products By Category
Supplier HomepageProductsincoloy alloysPrecipitation Hardening Nickel-Chromium Alloy with High Strength and Oxidation Resistance at Elevated Temperatures / Rene 41 /