Application: | Industrial |
---|---|
Standard: | GB, ASTM |
Purity: | >99.5% |
Alloy: | Alloy |
Powder: | Not Powder |
Transport Package: | Wooden |
Customization: |
---|
Suppliers with verified business licenses
MONEL K-500 alloy has corrosion resistance comparable to 400, but has higher mechanical strength and hardness. Has good thermal corrosion resistance and long-term tissue stability. It is mainly used in the manufacture of turbine blades and gas turbine blades with a working temperature below 750°C on aero-engines; used in the manufacture of fasteners and springs on ships; pump and valve parts on chemical equipment; doctor blades on papermaking equipment and so on.
Physical properties of MONEL K-500 alloy
Density: 0.318 lb/in3 / 8.80g/cm3
Elastic Modulus 26 000 ksi
Resistivity 5.11e-005 ohm-cm
heating energy 0.427 J/g-°C
thermal conductivity 22 W/m-°C
melting point 1300 - 1350 °C
magnetic 200H(At 70F)
Coefficient of Thermal Expansion, in./in./ F x 106
70-200F 7.7
70 - 400F 8.6
70 - 800F 8.9
70 - 1000F 9.1
Mechanical properties of MONEL K-500 alloy
Shape Tensile strength Yield Strength (0.2% Offset) Elongation,% Hardness
ksi MPa ksi MPa Brinell (3000-kg) RockwellB
Bar 70-90 482-621 25-60 172-413 45-30 110-170 60-86
Chemical composition of MONEL K-500 alloy:
alloy % nickel copper aluminum titanium iron manganese sulfur carbon silicon
Monle K500 minimum 63 27.0 2.30 0.35
maximum 33.0 3.15 0.85 2.0 1.5 0.01 0.25 0.5
,
Company Profile
Suppliers with verified business licenses