GH4037 (GH37) alloy is an austenitic aging-strengthened nickel-based alloy. Approximately 4% of aluminum and titanium are added to form a γ phase for aging strengthening, and more tungsten and molybdenum are added for solid solution strengthening, and a small amount of tungsten and molybdenum are added for solid solution strengthening. Boron strengthens the grain boundaries. The alloy is used below 850°C, has high thermal strength, good overall performance and structural stability, and is widely used in the manufacture of aero-engine turbine working blades, and is used for a long time below 800-850°C.
Similar grades:
Зи617 XH70BMTTЮ (Russia)
Chemical element content (%)
Ni Cr Fe C Mn Si Mo Al Ti V P Cu Ce B W S
Minimum Balane 13 0.03 2.00 1.70 1.80 0.10 5.00
Maximum Balane 26 5.0 0.10 0.50 0.40 4.00 2.30 2.30 0.50 0.015 0.07 0.020 0.020 7.00 0.010
Physical properties:
Density: 8.4g/cm3
Melting temperature range: 1278~1346ºC